About this product
ArmGrout M-80 HES is a single component pre weighed factory blended non-shrink, very high early strength free flow grout designed for very high early and final strengths. Its flow characteristics allow it to be used at various consistencies, and it is suitable for a wide range of loading situations.
Key features
- Excellent flow characteristics
- Low creep characteristics under sustained loading
- High early compressive, tensile and flexural strengths
- Non-shrink, ensuring complete surface contact and bond
- Suitable for a wide range of loading situations
- Chloride and iron free
Applications
- Heavy duty grouting requiring high early strength
Specifications
Form: Single component, pre weighed, factory blended | Water/Powder Ratio: 0.14 to 0.15 (Flowable) | Compressive Strength at 30°C (12 hrs): 15 N/mm2 (approx) | Compressive Strength at 30°C (1 Day): 40 N/mm2 (approx) | Compressive Strength at 30°C (3 Days): 60 N/mm2 (approx) | Compressive Strength at 30°C (28 Days): 80 N/mm2 (approx) | Compressive Strength at 25°C (1 Day): 30 N/mm2 (approx) | Compressive Strength at 25°C (3 Days): 60 N/mm2 (approx) | Compressive Strength at 25°C (28 Days): 80 N/mm2 (approx) | Compressive Strength Test Specimen: 70.6 mm x 70.6 mm x 70.6 mm cubes tested at 30°C (water curing after one day) | Controlled Expansion (plastic state): 1 - 4 % | Flexural Strength at 30°C (7 Days): 9 N/mm2 (approx), W/P ratio 0.15 (Flowable) | Flexural Strength at 30°C (28 Days): 10 N/mm2 (approx), W/P ratio 0.15 (Flowable) | Pot Life at 27°C: 15 minutes
Packing: 25 Kg HDPE bag