About this product

Contains selected graded dry sand, grey cement and imported and modified polymers; Superbond Technology improves workability, water retention, durability and adhesion. Joint thickness 3-4 mm against 10-12 mm for conventional mortar; curing not required.

Key features

  • High strength
  • Faster construction
  • No water percolation
  • Reduces wastage
  • Economical
  • No heat loss
  • Superbond Technology
  • Curing not required

Applications

  • Jointing of AAC blocks

Specifications

Joint thickness: 3 - 4 mm | Curing: Not required | Composition: Graded dry sand, grey cement, imported and modified polymers

Request a Quote

Get bulk pricing directly from the supplier.

Login to Request Quote
WHY BUY HERE
GST verified supplier
PAN & GSTIN checked by BrickoMart
Site delivery available
Coordinated with the supplier
GST invoice on every order
Full input tax credit
Quality-checked dispatch
Sourced from verified suppliers

More like this

Comparable products from verified suppliers

SITE Set delivery location
Home